BÖHLER N352S1 is a martensitic chromium steel with nickel addition. Heat treatable grade, capable of taking a mirror finish. Higher corrosion resistance compared to 13% chromium steel. Resistant to the effects of seawater, weak acids and alkaline solutions, as well as to acids having a strong, oxidizing effect such as nitric acid. Surface finish for optimum corrosion resistance: fine ground or polished.
For components subject to high mechanical and corrosive stress, e.g. screws and shafts, at operating temperatures up to approx. 752° F.
Martensitic chromium steel with nickel addition. Heat treatable grade, capable of taking a mirror finish. Resistant to the effects of seawater, weak acids and alkaline solutions, as well as to acids having a strong, oxidizing effect such as nitric acid. Surface finish for optimum corrosion resistance: fine ground or polished.
Others |
---|
BS : S80 |
C | Si | Mn | P | S | Cr | Mo | Ni | V | W | Cu | Co | Ti | Nb | Fe | Sn | |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
0.12 to 0.2 | max. 1 | max. 1 | max. 0.03 | max. 0.025 | 15 to 18 | max. 0.3 | 2 to 3 | max. 0.2 | max. 0.05 | max. 0.3 | max. 0.05 | max. 0.05 | max. 0.05 | REM | max. 0.02 |