A750

    Product Description

    BÖHLER Grade A750 is an austentic, corrosion and heat-resistant chromium nickel steel, niobium stabilized and solution treated. It have been used typically for parts requiring good corrasion resistance and which will be subjected to elevated temperatures during fabrication or in service and for parts requiring oxidation resistance up to 1500 °F (816°C),
    but usage is not limited to such applications. Compared to common 13% chromium steel, it offers higher corrosion resistance at lower strength and good weldability. No post-weld heat treatment required. The steel is resistant to atmospheric corrosion and the action of steam, water and acid as well as alkaline solutions. For optimum resistance, surfaces should be pickled. Cold forming properties are very good. The steel is capable of taking a mirror finish.

    Melting Route

    Airmelted

    Property Features

    Niobium stabilized, austenitic chromium nickel steel which resists intergranular corrosion in the temperature range up to 400°C (752°F). No post-weld heat treatment required. The steel is resistant to atmospheric corrosion and the action of steam, water and acid as well as alkaline solutions. For optimum resistance, surfaces should be pickled. Cold forming properties are very good. The steel is capable of taking a mirror finish.

    Technical Specifications

    Material Numbers


    1.4546 S34700 X5CrNiNb18-10 Z6CnNb1810


    Standards


    5646 S130 970 Pt.3

    Available product shapes

    • Long Products

      Long Products

    • Plates

      Plates

    Contacts

    BÖHLER Special Products

    Contact us!

    cancel
    cancel

    My account settings

    Please have a little patience. Your request is being processed.

    Please use a browser that is not outdated.

    You are using an outdated web browser.

    Errors may occur when using the website.